The finish is chosen from where the steel is going and how long it has to last — not from the price line. Here is how the decision is actually made, and what it does to your programme.

A fabricated steel frame loaded for delivery from the TMF Welding workshop

In this article

The short answer

The finish follows the site's corrosivity and the design life, not the cheapest line on the quote. Hot dip galvanising to AS/NZS 4680 suits exposed steel and anything hard to reach for maintenance. A paint system to AS/NZS 2312.1 suits interior, architectural and colour-matched work. A duplex system — galvanised, then painted — is for aggressive or coastal sites where appearance matters as well. Coastal South East Queensland is more corrosive than inland, and the difference is real.

Corrosion protection is the part of a steel package most often decided on price and most often regretted. The three common answers are galvanising, paint, and both. Which one is right is not a matter of taste — it comes out of two questions asked in order.

Question one: how corrosive is the site?

Australian sites are classified into atmospheric corrosivity categories, and the classification is what a coating system is selected against. AS 4312 maps corrosivity across Australia; the specifier, coatings consultant or engineer nominates the category for your site.

In South East Queensland the spread is wide. An internal frame in a suburban warehouse and a balustrade three hundred metres from open water at the Gold Coast are not the same problem, and a system that lasts decades on one will not last on the other. Distance from breaking surf, prevailing wind, whether the steel is sheltered or washed by rain, and whether it will ever be cleaned all move the answer.

Question two: how long does it have to last, and can anyone reach it?

Design life and maintenance access decide the rest. Steel that can be inspected and repainted from a ladder is a different proposition from steel above a roof line, inside a shaft, or behind cladding. If nobody is ever going to touch it again, the first coat has to do the whole job.

The three answers

Hot dip galvanising (AS/NZS 4680). The steel is dipped in molten zinc, so the coating covers inside and out, including edges and the inside faces of hollow sections. It is the durable default for exposed structural steel and for anything hard to get back to. It is not free of consequences: members have to be designed with vent and drain holes, the bath has a size limit so large members may need splicing, and heat distortion is a real thing on long slender pieces. All of that belongs on the shop drawings, not in a phone call after detailing.

Paint (AS/NZS 2312.1). A specified paint system — surface preparation, primer, build coats, topcoat — gives colour control and suits interior work, architectural steel and anything that has to match a palette. It depends completely on surface preparation, which is why the specification has to name the standard of blast cleaning, not just the paint.

Duplex, galvanised then painted. Galvanising under a paint system gives far more service life than either alone, and gives the finished colour as well. It is the answer for aggressive and coastal environments where the steel is also on show. It costs more and it takes longer, because the steel goes through two processes.

What the finish does to your programme

This is the part that catches builders out. Galvanising and painting are subcontracted processes with their own queues and their own transport legs. Steel leaves the workshop, goes to the coater, and comes back. That round trip is programme time, and it sits after fabrication and before delivery.

It also constrains the sequence. Galvanised steel that is site-welded loses its coating at the weld, and the repair has to be specified and done properly — AS/NZS 4680 covers repair of damaged galvanising, and a can of silver paint is not it. Where site welding is unavoidable, it is worth designing bolted connections instead, or agreeing the repair method before the steel leaves the shop.

Getting a comparable price

Two quotes for the same steel with different coating assumptions are not comparable, and coating is one of the easiest places for a price to look sharp. When you ask for a price, name the system or say plainly that you want the fabricator to nominate one and state it in the quote.

  • The corrosivity category or, at minimum, the site address and exposure
  • The design life the coating has to achieve
  • Whether colour matters, and to whose specification
  • Whether the steel can ever be maintained once it is up
  • Whether any connection will be welded on site
  • Who handles transport to and from the coater
  • Who does the touch-up after erection, and to what standard

Answer those seven and the coating line stops being a guess.

Common questions

Is galvanising always better than paint?

No. Galvanising is more durable in exposed conditions and covers surfaces a brush cannot reach, but it gives no colour control, imposes design requirements like vent and drain holes, and is limited by the size of the galvanising bath. For interior steel, or architectural steel that has to match a colour, a properly specified paint system is often the better answer.

What is a duplex coating system?

Hot dip galvanising with a paint system applied over it. The zinc does the corrosion work and the paint gives colour and an extra barrier. Service life is longer than either system used on its own, which is why duplex is common on coastal and aggressive sites where the steel is also visible.

Does structural steel in Brisbane need galvanising?

It depends entirely on where the steel sits. Sheltered internal steel in an inland suburb is a much lower corrosivity environment than exposed steel near open water. The site's corrosivity category, nominated against AS 4312, is what the coating system should be selected from — not a rule of thumb for the city as a whole.

What happens to galvanising when steel is welded on site?

The heat destroys the coating around the weld, and that area has to be repaired to the requirements of AS/NZS 4680 — normally with a specified zinc-rich product applied to a prepared surface. It is worth designing bolted site connections where you can, and agreeing the repair method in advance where you cannot.